New Findings on Atomic Layer Deposition from Korea Institute of Science and Technology Summarized (Electrochemical Assessment of Highly Reversible Sno2-coated Zn Metal Anodes Prepared Via Atomic Layer Deposition for Aqueous Zn-ion Batteries)

Press/Media: Press / Media

Period2023 Feb 22

Media coverage

1

Media coverage

  • TitleNew Findings on Atomic Layer Deposition from Korea Institute of Science and Technology Summarized (Electrochemical Assessment of Highly Reversible Sno2-coated Zn Metal Anodes Prepared Via Atomic Layer Deposition for Aqueous Zn-ion Batteries)
    Media name/outletSouth Korea Daily Report
    Country/TerritoryUnited States
    Date23/2/22
    PersonsSeung-Ho Yu