Abstract
Al conducting films are formed from the Al pastes with various amounts of glass powders. Pb-based glass powders with submicron size and spherical shape prepared by spray pyrolysis are used. The Al films formed from the Al pastes with high amount of glass powders have good adhesion properties with Si wafers. The optimum glass contents showing the minimum sheet resistance of the Al film changed according to the firing temperatures. The optimum glass contents are 7, 5 and 3 wt% of Al content at firing temperatures of 700, 800 and 900 °C, respectively. The minimum sheet resistance of the Al film with thickness of 31.4 μm is 9.5 mΩ/sq.
Original language | English |
---|---|
Pages (from-to) | 34-38 |
Number of pages | 5 |
Journal | Solar Energy Materials and Solar Cells |
Volume | 95 |
Issue number | 1 |
DOIs | |
Publication status | Published - 2011 Jan |
Externally published | Yes |
Keywords
- Electrical conductivity
- Electrode material
- Glass powder
- Spray pyrolysis
ASJC Scopus subject areas
- Electronic, Optical and Magnetic Materials
- Renewable Energy, Sustainability and the Environment
- Surfaces, Coatings and Films