Abstract
BaCu(B2O5) (BCB) ceramic powder was used to decrease the sintering temperatures of BaSm2Ti4O12 (BST) and BaNd2Ti5O14 (BNT) ceramics. The sintering temperature of the BST and BNT ceramics was reduced from approximately 1350 °C to 850 °C by the addition of BCB. The bulk density of the specimens increased and reached the saturated value with increasing BCB content. The variation of the dielectric constant (εr) was similar to that of the bulk density and, thus, the relative density plays an important role in determining the εr value of the specimens. The Q-value initially increased with the addition of BCB but decreased considerably when a large amount of BCB was added because of the presence of the liquid phase. Good microwave dielectric properties of Qxf = 4500 GHz, εr = 60 and τf = -30 ppm/°C were obtained for the 16.0 mol% BCB-added BST ceramics sintered at 875 °C for 2 h.
Original language | English |
---|---|
Pages (from-to) | 1868-1874 |
Number of pages | 7 |
Journal | Materials Research Bulletin |
Volume | 41 |
Issue number | 10 |
DOIs | |
Publication status | Published - 2006 Oct 12 |
Bibliographical note
Funding Information:This work was supported by the Ministry of Science and Technology through the Nano-Technology project. One of authors was financially supported by the Ministry of Science and Technology through NRL project.
Keywords
- A. Ceramics
- A. Electronic materials
- D. Dielectric properties
ASJC Scopus subject areas
- General Materials Science
- Condensed Matter Physics
- Mechanics of Materials
- Mechanical Engineering