Skip to main navigation Skip to search Skip to main content

Highly porous SnO2-SiO2 composite microspheres with interconnected pores for long-cycle-life lithium-Iion batteries

  • Soojin Han
  • , Seongmin Shin
  • , Suyeon Kim
  • , Hwidon Jeong
  • , Seung Yeop Han
  • , Dae Soo Jung
  • , Yun Chan Kang*
  • , Jung Hyun Kim
  • *Corresponding author for this work

Research output: Contribution to journal › Article › peer-review

Abstract

The simultaneous suppression of volume changes through pore structure design and the control of surface side reactions using passivating materials is critical for achieving high electrochemical performance and structural stability in lithium-ion battery anodes. In this study, highly porous SnO2-SiO2 composite microspheres with interconnected pores (p-SnSi) were prepared using a simple, one-step spray pyrolysis process. Fine and spherical polystyrene beads, which were burned off during the process, created a highly open and porous structure that extended throughout the inner bulk and surface. The highly open and porous structure effectively mitigated the mechanical strain induced by volume changes during the charge and discharge cycles of SnO2 while also providing a short lithium-ion diffusion length, thereby resulting in excellent electrochemical performance. Additionally, the SiO2 layer in p-SnSi suppressed surface side reactions on highly porous SnO2 with a large specific surface area, thereby enhancing the interfacial stability and contributing to improved cycling performance. The discharge capacities of the p-SnSi, filled structured SnO2-SiO2 composite microspheres (f-SnSi), porous SnO2 microspheres (p-Sn), and filled structured SnO2 microspheres (f-Sn) after 200 cycles at a current density of 1 A g−1 were 523 ± 12, 96 ± 6, 101 ± 9, and 59 ± 1 mA h g−1, respectively. Among these, p-SnSi demonstrated a higher lithium-ion storage capacity and capacity retention than f-SnSi, p-Sn, and f-Sn. In particular, the p-SnSi exhibited a stable reversible capacity of 544 ± 15 mA h g−1 after 500 cycles at a current density of 1 A g−1. These findings indicate that p-SnSi is a promising candidate for use in next-generation lithium-ion battery anodes.

Original languageEnglish
Article number139624
JournalJournal of Colloid and Interface Science
Volume706
DOIs
Publication statusPublished - 2026 Mar 15

Bibliographical note

Publisher Copyright:
© 2025

UN SDGs

This output contributes to the following UN Sustainable Development Goals (SDGs)

  1. SDG 7 - Affordable and Clean Energy
    SDG 7 Affordable and Clean Energy

Keywords

  • Anode materials
  • Lithium-ion batteries
  • Porous materials
  • Spray pyrolysis
  • Tin oxides

ASJC Scopus subject areas

  • Electronic, Optical and Magnetic Materials
  • Biomaterials
  • Surfaces, Coatings and Films
  • Colloid and Surface Chemistry

Fingerprint

Dive into the research topics of 'Highly porous SnO2-SiO2 composite microspheres with interconnected pores for long-cycle-life lithium-Iion batteries'. Together they form a unique fingerprint.

Cite this