STRESS CORROSION CRACK GROWTH OF HIGH DENSITY POLYETHYLENE WITH CRACKED ROUND BAR SPECIMEN IN CHLORINE MEDIUM

Jung Wook Wee, Alexander Chudnovsky, Byoung Ho Choi

Research output: Contribution to conferencePaperpeer-review